Elimination of the primary scale which has on its surface the as-cast product heated before being rolled.

This process is carried out with jets of water at high pressure and is of vital importance so that the hard and brittle scalel of the surface of the semiproduct does not adhere to the surface of the product during itshot rolling, avoiding from high roughness to holes.